Test item | Test method | Typical data |
Tensile strength | ASTM D2671 | ≥ 17MPa |
Breakdown elongation | ASTM D2671 | ≥ 500% |
specific gravity | ASTM D792 | 1.2 |
Tensile strength after aging | ASTM D2671 | ≥ 17MPa |
Breakdown elongation after aging | ASTM D2671 | ≥ 400% |
Heat shock | ASTM D2671 | 200/4h outer layer no drop no flow |
Low temperature flexibility | ASTM F2671 | -55/4h outer layer no cracking |
Volume Resistivity | ASTM D2671 | ≥ 1015Ω.cm |
Dielectric strength | ASTM D2671 | ≥ 20kV/mm |
Water absorption | ASTM D570 | ≤ 0.5% |
Copper corrosion | ASTM D2671 | pass |
Product Code | Wall thicknessafter free recovery(mm) | Standard Package(m/roll) |
A4-φ13/6 | 0.60 | 50 |
A4-φ19/7.8 | 0.75 | 50 |
A4-φ19/9.5 | 0.75 | 50 |
A4-φ21/7.8 | 0.75 | 50 |
A4-φ22/7.5 | 1.0 | 50 |
A4-φ25.4/9.5 | 0.70 | 50 |
A4-φ25/12.5 | 0.50 | 50 |
A4-φ30/15 | 0.50 | 50 |
A4-φ32/16 | 0.90 | 50 |
A4-φ35/17 | 0.50 | 50 |
A4-φ40/14 | 0.90 | 50 |
air conditioner tube