Ads by Google
Butyl Reclaimed Rubber:
Tensile Strength (MPA) | Elongation (%) | Ash Content (≤%) | Water content (≤%) | Density | Mooney Viscosity | |
9 MPA BUTYL Reclaimed rubber | 9 MPA | 460-480 | 10 | 1.05 | 1.10 | 50-90 |
12 MPA BUTYL Reclaimed rubber | 12 MPA | 500-550 | 9 | 1.00 | 1.05 | 50-90 |
excellent butyl reclaimed rubber