Activated Carbon for Gold Extraction
Series product for gold ore separation, Extracting the gold from gold ore with its high adsorption capacity,high-speed and lowest abrasion.
Specifications:
CIP Process | Heap Leaching Process | |
Iodine Value(mg/g) | 1000-1100 | 950-1100 |
Abrasion Resistance(%) | ≥99 | ≥98 |
Moisture(%) | ≤10 | ≤10 |
Paticial Size:
Mesh | Diameter(mm) |
A.8*16 | 1-2.38 |
B.8*20 | 0.84-2.38 |
C.8*30 | 0.59-2.38 |