Ads by Google
chemical composition and physicalproperties | |||||
\No. | 20#(ST45) | CK45 | 20Cr | 40Cr | 42CrMo |
C | 0.17-0.24 | 0.42-0.50 | 0.18~0.24 | 0.37-0.44 | 0.38-0.45 |
Mn | 0.35-0.65 | 0.50-0.80 | 0.50-0.80 | 0.50-0.80 | 0.50-0.80 |
Cr | <0.25 | <0.25 | 0.70-1.00 | 0.80-1.10 | 0.90-1.20 |
Si | 0.17-0.37 | 0.17-0.37 | 0.17-0.37 | 0.17-0.37 | 0.17-0.37 |
Ni | <0.25 | <0.25 | <0.030 | <0.30 | <0.030 |
Cu | <0.25 | <0.25 | <0.030 | <0.03 | <0.030 |
P | <0.035 | <0.035 | <0.035 | <0.030 | <0.035 |
s | <0.035 | <0.035 | <0.035 | <0.030 | <0.035 |
tensile strength | >410 | >600 | >835 | >980 | |
yield point | >245 | >355 | >540 | >785 | |
Brinell hardness | <156 | <229 | <179 | <207 |
:Ra ≤0.2 Micron and Rt≤2 Micron Tolerance on diameter: ISO f7Quality: half of the tolerance f7straightness: ≤0.2mm/m
Test in natural salt spray according to ASTM B 117-36 hoursPackage:seperate packed in tube,also according to your request
machined hard chrome plated CK45 or alloy steel piston rod