Epoxy Resin Impregnated Woven glass fiber tape
1) ISO9001-2000
2)High quality
3)High tensile strength
4)Excellent insumation
Epoxy Resin Impregnated Woven glass fiber tape:
Our company specializes in manufacturing of E-glass fiber tape,polyester filament tape,polyester filament and E-glass fiber interlace tape impregnated with polyester resin or epoxy resin.The tapes above mentioned are woven with yarns then impregnated with resins into semi-curing products. They are widely used as banding materials in the fields of transformer,reactor and lightning arrester, becoming good insulating matetrials for manufaturers. |
|
Property: |
Type | HY 750 | HY 740-1HY 740-2HY 740-3(Epoxy) | HY 741-1HY 741-2HY 741-3(Polyester) | Thermal class | H | F | F | Volatile content | ≤4% | ≤6% | ≤6% | Loss of weight at calcination | 29%±2% | 30%±2% | 30%±2% | Soluble resin content | ≥90% | ≥90% | ≥90% | Tensile strength before curing | Thickness(0.14mm)≥ 500N/cmThickness(0.20mm)≥ 800N/cmThickness(0.30mm)≥1000N/cm | Maximum pull while banding | Thickness(0.14mm)≥400N/cmThickness(0.20mm)≥700N/cmThickness(0.30mm)≥900N/cm |
|
Specification: |
Thickness (mm) | Width (mm) | Length (M/pancake) | 0.14,0.20,030 | 10,15,20,25,30,50 | 100, 150, 200 |
|
* Special specification and package are availabe upon request,(such as spool) |
Curing cycles: |
Temperature (°C) | 160 | 150 | 135 | 120 | 115 | Time(hour) | 4 | 5 | 8 | 16 | 24 |
|
* The above times do not include the time for the workpiece to reach the curing temperature. |
Storage stabiliy: |
Storage temperture °C | 0°C~20°C | 21°C~30°C | Time(day) | 60 | 45 |
|
Epoxy Resin Impregnated Woven glass fiber tape