Note:
PERMENDUR 2V PERMENDUR 49(HIPERCO 50A)
An alloy of 49% Cobalt, and 2%Vanadium, balance Iron. This alloy exhibits the highest magnetic saturation of any commercial alloy and excels in applications where this attribute is needed. This alloy has higher mechanical strength than other soft magnetic alloys.
Permendur is an alloy created by mixing 48-50% cobalt with iron (up to 2% vanadium can be added).It has a high permeability at high flux densities with a very high saturation point.Its magnetic transition temperature is 980°C.
Chemical Composition(%):
C≤0.04
P≤0.020
S≤0.020
Mn≤0.30
Si≤0.30
Ni≤0.50
Cu≤0.20
Co: 49.0~51.0
V: 0.80~1.80
Fe: Balance
Physical Property
Resistivity/(μΩ•m) : 0.40
Desinty(g/cm3): 8.20
Magnetostriction Coefficientλθ/10-6: 60-100
Tebsile Strength,N/MM2: Unannealed Annealed
1325 490
Applications
Electrical generators,pole pieces for electromagnets, magnetic bearings,and high magnetic flux devices and instruments.
Note: The values in the table are for reference only.
Specification: Plate, sheet, strip, rod, bar, wire, tube.
We are looing forward to cooperate with you!