Ads by Google
Material:Fluoroelastomer/FKM
Working temperature:-10°C ~200°C
FKM O-Ring Chemical Resistance Sheet
Hydrochloric acid 35% | A | Chloroform | A |
Sulfuric acid 98% | A | Trichloroethane | B |
Phosphate 85% | A | Methylene chloride | B |
Glacial acetic acid | D | Benzene | A |
Sodium hydroxide 80% | A | Toluene | A |
Ammonia 28% | A | Xylene | A |
Sodium hypochlorite 40% | A | Vinyl ether | D |
Acetone | D | Methanol | A |
Butanone | D | Ethanol | A |
Methyl isobutyl ketone | D | Isopropanol | A |
Carbon tetrachloride | A | Gasoline | A |
Trichloroethylene | A | Pure kerosene | A |
40°C×70 hr Volume change,
A 0~10%,B 10~20%,C 20~30%,D 30%
FKM O-ring