1. Powder feedthrough is vacuum-brazed with ceramic sleeves and metal parts
2. Ceramic sleeve was metallized with 95% alumina, 99% alumina etc,
3. Metal material is mainly stainless steel, kovar, Invar, Molybdenum and other rare alloy.
4. Weldarble type in assembly situation
5. Max Helium leak rate is less than 1×10-10Pa, tensile strength can be 120 MPa.
6. Voltage:3000V, Amperage: 12, 125, 250, 600 A