ITEM | SPECIFICATION | TEXT RESULT |
Grain number per gram | 30-70 | 39 |
Cleanness Per gram | 2 | ≤2 |
MFR g/10min | 9.0+1.0 | 9.1 |
tensile modulus( MPa) ≥ | 2500 | 2500 |
tensile yield strength (MPa) ≥ | 58 | 58 |
Exercise elongation % ≥ | 30 | 45 |
flexural strength (MPa) ≥ | 60 | 80 |
flexural modulus (MPa) ≥ | 2400 | 2550 |
Notched impact strength of the beam ≥ | 5.5 | |
1.8aMPa Load deformation temperature | 90 |