Ads by Google
we can supply ash 12%,min <60 ,8-14mpa reclaimed rubber and so on.please contact me for more information.
CERTIFICATE OF ANALYSIS OF 8MPA RECLAIMED RUBBER
SI.NO. | PARAMETER | UOM | SPECIFICATION |
1. | APPEARANCE | - | BLACK RUBBER SHEET |
2. | SPECIFIC GRAVITY AT RT | - | 1.10-1.20 |
3. | ASH CONTENT | % | 12 |
4. | WATER CONTENT | % | 1.2MAX |
5. | ACETONE EXTRACT | % | 16 |
6. | MOONEY ML1+4 (AT 100°C) | % | <60 |
7. | TENSILE STRENGTH(AT 145°C/15) | MPA | 8.0 |
8. | ELONGATION AT BREAK | % | 280 |
9. | CARBON BLACK BONTENT | % | 28-30 |
10. | RUBBER HYDRO CARBON CONTENT | % | 48-52 |
11. | STANDARD PACKING | KG | 20KG/PIECE |
uncured compound rubber for conveyor belt