Ads by Google
AZS Fused Cast Skew Block Used in Charging Hole,Crater of Glass Furnace.
AZS refractories are used for melting glass furnaces, can stand aggressive conditions in contact with molten glass.
The different content of ZrO2 led to three model: AZS33#, AZS36#,AZS41#.
Our company produce the AZS Fused Cast Refractories as per different use and customer requirement.
We have four casting method: Normal casting;
Tilt casting;
Semi-Void-Free casting;
Void-free casting.
Item | Index | |||
AMZ33# | AMZ36# | AMZ41# | ||
Chemical Composition(%) | Al2O3 | Margin | Margin | Margin |
ZrO2 | 32.0-34.5 | 35.0-37 | 40.0-42.0 | |
SiO2≤ | 15.5 | 14 | 13 | |
Fe2O3≤ | 0.1 | 0.1 | 0.1 | |
TiO2≤ | 0.05 | 0.05 | 0.05 | |
Na2O≤ | 1.5 | 1.4 | 1.3 | |
Physical Composition | Apparent Porosity(%) | 2 | 1.5 | 1.3 |
Bulk Density(g/m³) | 3.8 | 3.89 | 4.12 | |
Cold Crushing Strength(MPa) | 350 | 350 | 350 | |
Refractorlness(°C) | 1710 | 1710 | 1730 | |
0.2MPa Softening temp. Under load(°C) | >1700 | >1700 | >1700 | |
Exudation temp. of Glass Phase(°C) | >1400 | >1420 | >1430 | |
Corrosion Resistance of Glass Melt (mm/24h) | 1.3 | 1.2 | 1.1 | |
Thermal Expansion(%) | 0.8 | 0.8 | 0.8 | |
Glass Phase(%) | 20 | 19 | 18 | |
Bulk Density(g/m³) | PT.QX | 3.4 | 3.45 | 3.55 |
ZWS | 3.6 | 3.65 | 3.9 | |
WS | 3.7 | 3.78 | 3.92 |