1.Type analysis
C | Si | Mn | Cr | Mo | Ti | Fe | S | Co | Ni |
0.015 | 0.08 | 1.0 | 14-18 | 14-17 | 0.7 | 3 | 0.030 | 2.0 | balance |
2.Description
HASTELLOY C-4 alloy is a nickelchromium- molybdenum alloy with outstanding high-temperature stability, as evidenced by high ductility and corrosion resistance even after longtime aging at 1200 to 1900 deg. F (649 to 1038 deg. C). The alloy also has excellent resistance to stress corrosion cracking and to oxidizing atmospheres up to 1900 deg. F (1038 deg. C).
Hastelloy C-4 /N06455 superalloy wires