Ads by Google
Style | Chinese standard | U.S.A(AWS) | Japan(JIS) | Dia(φmm) | Rockwell hardness(HRC) | Melt the deposited metal main chemical composition(%) | Main Usage | ||||
C | Mn | Si | S | P | |||||||
LY 502Ni |
|
|
| 1.2 /1.6 | ≥35 | ≤0.50 | - | - | - | - | Used for surfacing welding between metal wear and mild sand wear parts. |
LY R402 |
|
|
| 1.2 /1.6 | ≥35 | 0.12 | 1.50 | 0.51 | 0.014 | 0.019 | Used in metal wear and the sand wear parts between the hardfaced surfacing, it contains the golden section, except Cr outside also contain Mo, V elements of tempering softening properties, relatively strong, can get stable hardness. |
Wear-resistant overlaying flux-cored welding wire