Ads by Google
Especially insensitive to oil, rust, scale, dirt and primers on the surface to be welded. Slag detachability in narrow groove and resistance to porosity are excellent. As the consumption of flux is very small, it is very economical.Applicable to horizontal and flat fillet welding.
Notes on Usage
1,Dry the flux at 300~350 (572~662 ) for 60 minutes before use.2,When the flux height is excessive, poor bead appearance may occur.3,Remove rust, scales, oil, paint, water, dirt and slag of tack welds from the groove to obtain sound weld metal.4,Use welding current and speed as low as possible at the first layer of groove to avoid cracking.
HYUNDAI Brand welding